dc.description.abstract An attempt bas been made to correlate two important factors in the design of soil-cement pavements, namely, California Bearing Ratio and Shear Strength. Three mixes A, B and C were prepared using locally available Ranipur sand (fine sand) and olay in three proportions. In mixes A, B and C the percentages of clay to sand were 10, 20 and 30 respectively. The samples in the C.B.R. testing mould and for triaxial shear test were pre-pared using .0, 4, 8 and 12 percent' cementfor the above three mixes at optimum moisture content. The samples were cured in moist condition for three days and then soaked for another four days under water. The tests were carried out in C.B.R. testing biaciline. In the triaxial shear machine, 10, 20, 30 and 40 psi. confining pressures were used. The strength parameters 'C' and were obtained from these tests. The C.B.R. values and cohesion for each sample were plotted on a double logarithmic graph and were found to follow a straight line relationship for equal percentages of cement. The value of • 1) ' for all the three mixes increased slightly with ()emelt percentage, irregularly and was assumed to be practically constant. I. en_US
dc.language.iso en en_US
dc.subject CIVIL ENGINEERING en_US
dc.subject CO..B.R. W11TH SHEAR STRENGTH en_US
dc.subject SHEAR STRENGTH en_US
dc.subject CEMENT SLUMMED SORLS en_US
dc.title CORRELATRON OF Co.B.R. W11TH SHEAR STRENGTH OF CEMENT SLUMMED SORLS en_US
dc.type Doctoral Thesis en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record