CHARACTERISTICS OF COLD WORKED AL-SI SPRAY FORMED PARTS

Show simple item record

dc.contributor.author Rajpoot, Rajesh
dc.date.accessioned 2014-11-25T06:12:18Z
dc.date.available 2014-11-25T06:12:18Z
dc.date.issued 2010
dc.identifier M.Tech en_US
dc.identifier.uri http://hdl.handle.net/123456789/10876
dc.guide Singh, Devendra
dc.description.abstract Al alloys has high strength, low density, good wear resistance, low coefficient of thermal expansion. Its low density, which can contribute significantly to the aspect of weight savings in the design and construction of automotive and aerospace components, materials handling equipment, portable tools and even sporting goods. These properties can be improved by the mechanical processing. By these processes mechanical properties such as ultimate strength, yield strength and percentage elongation and microstructure of the Al alloy may be improved.A rolling thickness reduction of 5% produces Al—Si strip having optimum properties. The mechanism of densification in the deposit layer during rolling has been discussed on the basis ofthe examination of the microstructure of the deposit at different stages of rolling. It is obserbd that the wear behaviour is affected by varios mechanical properties The wear behaviour is also dependent on the load and hardness. en_US
dc.language.iso en en_US
dc.subject AL-SI SPRAY en_US
dc.subject WEAR BEHAVIOUR en_US
dc.subject MECHENICAL PROPERTIES en_US
dc.subject METALLURGICAL AND MATERIALS ENGINEERING en_US
dc.title CHARACTERISTICS OF COLD WORKED AL-SI SPRAY FORMED PARTS en_US
dc.type M.Tech Dessertation en_US
dc.accession.number G20477 en_US