dc.description.abstractAustenitic stainless steel pipes are available in different grades according to their intended applications. In this investigation, AIS 304LN austenitic stainless steel pipes having 25 mm thickness and 300 mm inner diameter with conventional and narrow groove were welded by GMAW and P-GMAW process. GTAW process was used for the root pass. Effect of GMAW and P-GMAW process parameters on transverse shrinkage and shrinkage stresses were measured. Comparison of shrinkage and shrinkage stresses were done on conventional groove with GMAW and P-GMAW process and narrow groove by P-GMAW process. It is observed that narrow groove weld design with controlled welding parameters can improve the weld joint characteristics with respect to the transverse shrinkage and shrinkage stresses.en_US
dc.description.sponsorshipINDIAN INSTITUTE OF TECHNOLOGY ROORKEEen_US
dc.language.isoenen_US
dc.publisherI I T ROORKEEen_US
dc.subjectAustenitic Stainless Steelen_US
dc.subjectShrinkage Stressesen_US
dc.subjectSteel Pipesen_US
dc.subjectDifferent Gradesen_US
dc.titleMINIMIZING THE TRANSVERSE SHRINKAGE AND SHRINKAGE STRESSES IN AUSTENITIC STAINLESS STEEL MULTIPASS THICK PIPE WELDSen_US
dc.typeOtheren_US
Appears in Collections:MASTERS' THESES (MIED)

Files in This Item:
File Description SizeFormat 
G22572.pdf8.3 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.